Posted in

How to ensure the color fastness of thermoforming film?

If you’ve ever walked past a newly molded thermoformed part—say, a disposable food container, a clamshell for electronics, or a custom plastic tray for medical devices—and noticed faded patches, streaks, or color bleeding after just a few uses or even during production, you know how much a color fastness issue can derail your project. As a thermoforming film supplier with over 12 years in the business, I’ve had countless conversations with clients who thought their only options were to accept a subpar batch, rework the entire run, or eat the cost of materials. The truth is, color fastness in thermoforming films isn’t a lucky guess or a fluke—it’s a combination of intentional material selection, precise processing, and rigorous quality checks that start long before the first sheet ever goes into a thermoformer. Let me walk you through what I’ve learned, the mistakes I’ve helped clients fix, and the steps we take at our facility to make sure every film we ship holds its color, no matter what it’s up against. Thermoforming Film

First, let’s get clear on what “color fastness” actually means for thermoformed parts. It’s not just about looking good—though that’s obviously a big part of brand consistency for retail packaging, medical devices, or printed promotional items. For food-grade thermoforming films, color fastness means no bleeding when the part comes into contact with hot food oils, acidic sauces, or microwaving. For industrial parts, it means no fading when exposed to UV light, harsh cleaning chemicals, or long-term storage in warehouse conditions. For medical packaging, it even means the color won’t transfer to sterile equipment or interfere with diagnostic testing. All of these are non-negotiable, and as a supplier, my job is to make sure our films are engineered to meet those specific requirements, not just a generic color “test.”

The foundation of good color fastness starts with the pigments and dyes we choose during film formulation, and this is where a lot of less experienced suppliers cut corners. I’ve seen clients come to us with films they bought from a competitor that faded within a week of being displayed on store shelves, and when we tested the pigments, we found they were cheap, low-melting dyes that couldn’t withstand the high temperatures of thermoforming. Thermoforming typically involves heating a film to between 160°C and 260°C, depending on the plastic type (PET, PP, PS, or PVC, to name the most common), and if the pigment isn’t designed to hold up at those temps, it breaks down during heating. Even worse, some pigments are not “migration-resistant”—meaning they can leach out of the film when it’s exposed to certain substances, which is a big no-no for food and medical applications.

At our facility, we only use pigments that are specifically formulated for thermoforming processes, and we categorize them by their intended use case. For example, if a client needs a film for a cold-formed medical tray that will go through sterilization, we use high-performance, non-migrating metal complex pigments that won’t bleed when exposed to ethylene oxide or autoclave heat. For a retail food container that will be microwaved, we choose heat-stable pigments rated to withstand up to 280°C for short periods of time, plus ones that are FDA-compliant to prevent transfer to food. For outdoor thermoformed parts like patio furniture trims or landscape signage, we use UV-stabilized pigments that resist fading from sun exposure, which is a feature we actually flag clearly in our product spec sheets—no fine print. The key here is that pigments aren’t a one-size-fits-all, and as a supplier, we don’t just pick whatever color is cheapest; we match the pigment to the end use to build in color fastness from the start.

Next, the base resin of the film plays a huge role in how pigments adhere and stay locked in. I can’t tell you how many times a client has said, “We used the same color as last year, but this year it’s fading,” only to realize they switched from a PET resin to a cheaper, lower-grade PP resin to save money. Resins have different molecular structures, and some are more porous or have lower melting points than others, which affects how well pigments disperse and bond to the film. For example, PP is a non-polar resin, which means it doesn’t mix well with polar pigments—if you don’t adjust the pigment formulation or add a compatibilizer during film extrusion, the pigments can clump together or separate from the resin during thermoforming, leading to uneven color or fading.

At our plant, we work closely with resin manufacturers to pre-test how our pigment blends interact with different resin types before we even produce a batch for a client. If a client is using PP for their thermoformed parts, we don’t just add red pigment to the PP resin—we adjust the pigment load and add a small amount of a maleic anhydride compatibilizer to ensure the pigments are uniformly dispersed and bonded to the PP molecules. For PET films, which are polar, we use a different compatibilizer to keep pigments from settling during the extrusion process, which leads to consistent color across the entire sheet, even after deep thermoforming where the material stretches up to 300%. We also do what’s called a “film adhesion test” for every batch: after extruding a sample sheet, we apply tape to the surface, pull it off, and check for pigment transfer. If even a tiny amount of color comes off on the tape, we adjust the formulation before shipping, because that’s a sign of poor color fastness waiting to happen.

Once the film is formulated and produced, the thermoforming process itself is a make-or-break step for color fastness. I’ve worked with clients who had amazing films that faded during thermoforming because they cranked up the heat too high, too fast, or left the film in the oven for too long. Even if the pigment is heat-stable, excessive heat can cause the resin to break down, which in turn breaks down the pigment bonds. Conversely, if the film isn’t heated evenly, some areas of the part will stretch more than others, and the pigment concentration can become thinner in those stretched areas, leading to lighter, faded spots. That’s a problem I see all the time with deep-draw thermoformed parts, like large storage bins or automotive interior trim, where the corners stretch the most.

As a supplier, we don’t just hand over a roll of film and disappear—we offer process guidance tailored to each client’s specific needs. For example, if a client is thermoforming a deep-draw PET food container, we’ll tell them to use a radiant oven with zone heating, not just a single heat setting, so the film heats evenly from top to bottom, and the corners get the same amount of heat as the flat edges. We also recommend a forming temperature between 180°C and 200°C for that application, instead of the 250°C a less experienced thermoformer might use, which would cause pigment degradation. For clients using PS films for disposable clamshells, we advise them to avoid direct contact between the hot film and metal tooling, because that can cause localized overheating and pigment discoloration. We even provide a step-by-step process cheat sheet for every product we sell, with specific temperature ranges, dwell times, and pressure settings, because we know that even the best film in the world will fail if it’s run through a thermoformer incorrectly.

Another critical, often overlooked, factor is the post-thermoforming treatment. A lot of clients think once the part is formed, they’re done, but additional processes like trimming, stacking, or applying labels can affect color fastness if not done right. For example, if a client uses a hydraulic press to trim excess material from a thermoformed part, the sharp blades can generate friction and heat that can scorch the pigment along the trim edge, leading to faded or discolored lines. Or if they stack parts too tightly right after thermoforming, residual heat can get trapped, causing the pigment to migrate between parts, especially if the parts are still warm. For clients doing high-volume production, we recommend using a cold trimming process with a laser cutter instead of a hydraulic press, because laser trimming is precise and generates less heat, leaving the edges with the same color as the rest of the part. For smaller batches, we advise letting parts cool completely for at least 24 hours before stacking or handling them, which gives the pigment-resin bonds time to fully set and prevents migration.

We also have a rigorous quality control (QC) process here at our facility that includes color fastness testing before any film leaves our dock. I’m a big believer in testing real-world conditions, not just lab tests, because a color that passes a 24-hour lab UV test might fail after 6 months of being displayed in a store window with direct sunlight. For every custom film order, we run three key color fastness tests: a heat stability test, a migration test, and a UV resistance test. The heat stability test involves taking a sample of the film, heating it to the maximum forming temperature specified by the client for 5 minutes, then comparing the color to an unheated sample using a spectrophotometer—if the color difference is more than 1 delta E (the standard for industrial color consistency), we rework the batch. The migration test involves placing a film sample in contact with the food simulant specified by the client (like 3% acetic acid for acidic foods, or mineral oil for fatty foods) and storing it at 40°C for 10 days, then checking for color transfer to the simulant. For UV resistance, we use a xenon arc weatherometer to expose samples to 1000 hours of UV light, which is roughly equivalent to 1 year of outdoor sun exposure, and measure fading again with the spectrophotometer. We keep all test records for every batch we produce, so if a client has a question about a specific order, we can pull up the test data immediately—no excuses.

I’ve learned over the years that the best way to avoid color fastness issues is to be transparent with clients from the start. I don’t oversell a film as “perfect for every application” if it’s not, and I always warn clients if we need to adjust a formulation to meet their specific needs. For example, a few years ago, a startup company came to us with a design for custom thermoformed trays for plant-based meat packaging. They needed the trays to be FDA-compliant, resist color bleeding when in contact with raw meat juices, and have a bright red logo that wouldn’t fade during shipping and storage. Initially, we offered our standard FDA-compliant red pigment, but when we ran the migration test, we found that the red pigment leached slightly into the meat simulant, which wasn’t acceptable for their product. Instead of just selling them the film they asked for, we worked with our pigment supplier to adjust the pigment blend, adding a special polymer coating around each pigment particle to lock it in, and ran multiple tests until we had a red pigment that passed both the FDA migration test and the UV resistance test. The client ended up being one of our repeat customers, and they told us their color fastness was the main reason they chose us over other suppliers they’d tried in the past.

That experience reinforced for me that color fastness isn’t just a technical detail—it’s a way to build trust with your clients. If your thermoformed parts fade or bleed, it doesn’t just reflect badly on you as a manufacturer; it hurts the brand of the client who’s using your film. As a supplier, that’s my responsibility: to make sure every film I send out has the best possible color fastness, no matter how small the order or how specific the requirements.

If you’re currently dealing with color fastness issues with your thermoformed parts, or if you’re looking for a reliable supplier that prioritizes color consistency, I’d be happy to talk through your project. We work with clients across industries—food packaging, medical devices, industrial components, retail display—and we can help you select the right film, adjust your process, and test to make sure your final parts hold their color. Whether you need a small custom batch for a new product launch or high-volume production for a national brand, we have the expertise to get it right.

Bulk Liquid Bags References:

  1. Andrews, J. (2021). Color Fastness in Thermoplastic Films: Formulation and Processing Considerations. Journal of Plastic Film & Sheeting, 37(2), 145-162.
  2. European Committee for Standardization. (2019). Plastics – Thermoforming Films – Test Methods for Color Fastness. EN 15535:2019.
  3. Food and Drug Administration. (2022). Guidance for Industry: Use of Color Additives in Food Contact Materials. U.S. FDA Center for Food Safety and Applied Nutrition.
  4. Lopez, M. (2020). Pigment Selection for High-Temperature Thermoforming Applications. Pigment & Resin Technology, 49(4), 211-218.

Haining Huilong Plastic Co., Ltd.
Haining Huilong Plastic Co., Ltd. is one of the most professional thermoforming film manufacturers and suppliers in China, featured by quality products and good service. Please rest assured to wholesale bulk customized thermoforming film made in China here from our factory.
Address: No.6 DanFeng Road, Haining, Jiaxing City, Zhejiang Province
E-mail: info@huilongplastic.com
WebSite: https://www.huilongplastic.com/